trilithium nitride


Solid Phase Heat Capacity (Shomate Equation)

Go To: Top, References, Notes

Data compilation copyright by the U.S. Secretary of Commerce on behalf of the U.S.A. All rights reserved.

Cp° = A + B*t + C*t2 + D*t3 + E/t2
H° − H°298.15= A*t + B*t2/2 + C*t3/3 + D*t4/4 − E/t + F − H
S° = A*ln(t) + B*t + C*t2/2 + D*t3/3 − E/(2*t2) + G
    Cp = heat capacity (J/mol*K)
    H° = standard enthalpy (kJ/mol)
    S° = standard entropy (J/mol*K)
    t = temperature (K) / 1000.

View plot Requires a JavaScript / HTML 5 canvas capable browser.

Temperature (K) 298. - 1300.
A 54.92462
B 86.21550
C 8.427957
D -8.103656
E -0.521293
F -186.5499
G 100.1871
H -164.5571
ReferenceChase, 1998
Comment Data last reviewed in March, 1978
Temperature
(K)
Cp
(J/mol*K)

(J/mol*K)
-(G° - H°298.15)/T
(J/mol*K)
H° - H°298.15
(kJ/mol)
298.75.2862.6262.590.01
300.75.5463.1362.590.16
400.86.9886.4865.718.31
500.97.04107.071.9617.51
600.106.5125.579.3627.69
700.115.6142.687.1938.80
800.124.3158.695.1350.80
900.132.8173.8103.063.65
1000.140.9188.2110.877.34
1100.148.7202.0118.591.83
1200.156.2215.2126.0107.1
1300.163.1228.0133.4123.0

References

Go To: Top, Solid Phase Heat Capacity (Shomate Equation), Notes

Data compilation copyright by the U.S. Secretary of Commerce on behalf of the U.S.A. All rights reserved.

Chase, 1998
Chase, M.W., Jr., NIST-JANAF Themochemical Tables, Fourth Edition, J. Phys. Chem. Ref. Data, Monograph 9, 1998, 1-1951. [all data]


Notes

Go To: Top, Solid Phase Heat Capacity (Shomate Equation), References