Quantity Value Units Method Reference Comment
solid,1 bar70.27cal/mol*KN/ALebedev, Lebedev, et al., 1981glass phase; Highly elastic state.
solid,1 bar70.27cal/mol*KN/ALebedev, Lebedev, et al., 1979glass phase

Constant pressure heat capacity of solid

Cp,solid (cal/mol*K) Temperature (K) Reference Comment
74.21298.15Lebedev, Lebedev, et al., 1981glass phase; T = 5 to 330 K. Highly elastic state.
74.21298.15Lebedev, Lebedev, et al., 1979glass phase; T = 9 to 330 K.

References

Go To: Top, Condensed phase thermochemistry data, Notes

Data compilation copyright by the U.S. Secretary of Commerce on behalf of the U.S.A. All rights reserved.

Lebedev, Lebedev, et al., 1981
Lebedev, B.V.; Lebedev, N.K.; Khotimskii, V.S.; Durgar'yan, S.G.; Nametkin, N.S., Thermodynamics of polymerization of vinylorganosilanes, Dokl. Akad. Nauk, 1981, SSSR 259, 629-633. [all data]

Lebedev, Lebedev, et al., 1979
Lebedev, N.K.; Lebedev, B.V.; Khotimskii, V.S.; Durgar'yan, S.G., The calorimetric study of vinylbenzyldimethylsilane, polyvinylbenzyldimethylsilane and the process of vinylbenzyldimethylsilane polymerization in the region 9 to 330 K, Vysokomol. Soedin., Ser., 1979, A 21, 1031-1036. [all data]


Notes

Go To: Top, Condensed phase thermochemistry data, References